yes, the laminator is a major step up in getting a good transfer and the foil does help.
I spent the last 2 days ironing out the same pattern at home but couldn't get it even.
with the laminator, it took just 5 mins.
apparently if it reaches 150 to 160deg c, you can get it transferred in one pass.
the one I have at work is just a normal one but with a heat setting from 1 to 10, so I could set it at max.
the 0.8mm pcb is also important though as it gets through the rollers without jamming.
i'm sure a double sided pcb is possible this way as well. that's my next one.
|