Sounds like a good idea. Galvanising is good for 15 years in regular contact with water or occasional salty spray . That is halved in constant contact with concrete or salty water.

So if it gets wet or salty constantly, galvanised , two part primed, painted and/ or damp proof the concrete. Acrylic paint will not adhere to galvanising but on a two part primer it is still best to use a solvent based top coat.